Injection molding machine mold parts Maintenance Considerations

Date:2016-06-24 13:22:52

The required injection molding machine injection molding die each year position maintenance procedures, depending on the mold cycle. Here are some maintenance tips injection molding machine mold parts, injection molding machines allows each user to ensure the effective operation of the mold hot runner heater, guide posts and thimble, molding inserts injection molding machine mold assembly to prevent accidental circumstances occur.
1. Check whether the injection molding machine at the aeration holes have early warning of rust or damp phenomenon.
If you find the hot runner near the discharge vent rust or damp phenomenon, it means that internal condensation, or water may be broken in the injection molding machine. Damp phenomenon will lead to the injection molding machine heater fatal short circuit. If the machine is not running endlessly throughout the year, we need to shut down in the evenings or weekends, then this occurs the injection molding machine will increase the chance of condensation.
2. Remember to alert the operator not to heat the nozzle head at the gate of the injection molding machine "clean" out.
If the operator happen to see die at the outlet of a small piece of stainless steel, there may be a point nozzle assembly. "Clean up" out of this seemingly impeding things often ruin head hot mouth. In order not to destroy the hot mouth, please before taking action to confirm the type of nozzle head hot runner system, and to ensure that all operators are well trained and can identify different types of mouth own head contact.
3. The injection molding machine sliding stop button
For the year endlessly running injection molding machines, this work should be done once a week. And the end is a very good opportunity to give these parts a routine lubrication and maintenance.
4. The resistance value of the injection molding machine interaction check heater
You should just start using the injection molding machine heater when it had measured the resistance, but at the end it is again measured and compared to their time. If the resistance values ​​are ± 10% of the float should consider getting a replacement heater injection molding machines, to ensure that it does not fail at the critical moment of the production process. If it has never been measured initial resistance value, so now measured once, and the resulting value is used as a reference for future examination of the data when the heater.
5. Check the injection molding machine and injection molding machine guide pin guide bush whether there are signs of wear
Looking for scratches or abrasions and other traces of mold parts that wear due to lack of lubrication caused. If traces only just appear, you can also give the injection molding machine and injection molding machine guide pin guide sleeve plus lubricant to prolong its life. If wear is very serious, it should be replaced with new parts up. Otherwise, the cavity and core portions may not be a good fit, resulting in different parts of the cavity wall Bohou.
6. Check the flow of water injection molding machine
Connect a hose in an injection molding machine at the exit of the waterway, to let the water through the pipes to the bucket. If you do not clear out of the water or the color, there might be rusty phenomenon, which means that the water is not smooth blockage somewhere. If you find that these issues will be drilled through all the pipes again (or you take any of the methods most commonly used to clean up), in order to ensure the smooth flow. Improved plant's water treatment system that can prevent the emergence of various problems caused by the rust and blocking future.
7. Clean the injection molding machine thimble
After a year's time, thimble and a film due to gas accumulation of impurities becomes dirty. Recommended by injection molding machine mold cleaning agent to take some cleaning every 6-12 months. Clean, and then coated with a layer of lubricant on the thimble to prevent scratches or breakage.
8. Check whether the injection molding machine hot mouth radius fracture region
Fracture by remaining in the injection molding machine hot mouth loose hardened plastic debris by clamping force from the cartridge assembly in the forward injection caused. Cause of the problem is also possible that the centerline is not aligned. When the fracture was found, to consider both possibilities. If you have suffered damage severe enough to prevent leakage when the petals (a term injection mold machine formerly used by the user, means between the thermal head in the mouth of the guide sleeve and the emergence of machine plastic leak), it should be replaced sprue bushing .

Return

Copyright:TAYU Machinery Co.,Ltd.  Address:Xianlin Industrial Zone, Yuhang, Hangzhou, China  技术支持:中国机械网
TEL:0086-571-88687296  FAX:0086-571-88686887  Email:sales@tayu.cn 浙ICP备10018881号

TAYU Injection Molding Machine Product: injection molding machine vertical injection molding machine bakelite injection molding machine BMC injection molding machine rubber injection molding machine insert injection molding machine